LOCTITE Nordbak Wearing Compound™ - The Wercs
TDS LOCTITE® Nordbak® Wearing Compound™, July-2015 Mixing: 1. Measure 2 parts resin to 1 part hardener by volume or weight, transfer entire kit onto a clean and dry mixing surface and mix together until uniform in color. 2. If resin and hardener temperatures are 15 °C or below, preheat resin only to about 32 °C but not to exceed 38 °C.